Mordanting Cellulose Fiber Part 1: Tannin Bath

You must first complete Introduction before viewing this Lesson
Please sign up for the course before starting the lesson.

Apply Tannin *Use 10% WOG to measure the amount of tannin needed Example: 10% x WOG= grams of tannin 10% x 100gms = 10gms of tannin -Dissolve tannin in a pot of hot/warm water with enough water to allow the fibers to move freely. -Soak the fibers for 1-2 hours, allowing the bath to cool …